DESOI AnchorNox® dry mortar

Vorteil/Hinweis
  • Good fl owability
  • Cement bound and free of chloride
  • Controlled volumination with non-positive connection
  • High early and ultimate strength, high bond strength
  • Compressive strength after 28 days > 34.7 N / mm2
  • Low w / c ratio
Technische Daten
Grain size 0 - 0.5 mm
Water demand 2.6 - 2.7 l
Consistence well flowing
Fresh mortar raw density (DIN EN 1015-11) approx. 2.0 kg/ dm³
Compressive strength (DIN 1015)
after 1 day > 0.5 N/mm²
after 7 days > 27.0 N/mm²
after 28 days > 41.5 N/mm²
Bending tensile strength N/mm²
after 1 day > 0.5 N/mm²
after 7 days > 5.1 N/mm²
after 28 days > 7.4 N/mm²
Processing time approx. 45 minutes (20°C)
Swelling tolerance + 0,3 Vol. %/24 h
The stated strength values are average values.
Produktbeschreibung
DESOI AnchorNox ® dry mortar is suitable for the injection and filling of anchor systems, e. g. the DESOI anchor stocking system, anchorages in rock, concrete and masonry.